DSpace at Transilvania University >
Mechanical Engineering >
COMEC 2009 >
Please use this identifier to cite or link to this item:
http://hdl.handle.net/123456789/1163
|
Title: | MECHANICAL CHARACTERISTICS FOR COBALT - CHROMIUM AND NICKEL - CHROMIUM CAST ALLOYS RECOVERY |
Authors: | ROSCA, Daniela ROSCA, Adrian PITRU, Allma Roxana |
Keywords: | mechanical characteristics, Co-Cr and Ni-Cr cast alloys, recovery |
Issue Date: | 2009 |
Publisher: | Transilvania University Press of Braşov |
Citation: | Google Scholar |
Series/Report no.: | COMEC 2009;633-636 |
Abstract: | Since cobalt-chromium or nickel-chromium casting alloys became available for cast removable partial-denture
restorations, their popularity have continued to increase. It was estimated that more than 80% of all partial-denture
appliances were cast from cast from some type of these of base-metal alloy.
According ANSI/ADA the specification of these dental restorative materials has to indicate the comply satisfactorily with
requirements on toxicity, hypersensitivity, and corrosion of elemental composition, and the required minimum values for
elongation, yield strength, and elastic modulus.
The paper presents experimental considerations (experimental diagrams and values) concerning the possibility to recovery
the cobalt-chromium and nickel-chromium alloys after the first casting. |